REFRACTORY GRAINS OF CORUNDUM BROWN
|
| A block of Corundum Brown is smelted from calcinated bauxites, cokes and Fe cuts in arc electrical furnace. From that block, lump of I. grade is sorted out, milled on roll crusher, magnetized, annealed at temperature of 1050 oC and sieved according to a required granulometrical composition.
|
guaranteed analysis |
Al2O3 |
95,0 % min. |
Fe2O3 |
0,3 % max. |
TiO2 |
3,0 % max. |
SiO2 |
1,0 % max. |
granulation | g/dm3 min. | granulation | g/dm3 min. |
F12 | 2010 | F60 | 1750 |
F14 | 1980 | F70 | 1730 |
F16 | 1970 | F80 | 1720 |
F20 | 1950 | F90 | 1700 |
F24 | 1900 | F100 | 1680 |
F30 | 1870 | F120 | 1650 |
F36 | 1850 | F150 | 1600 |
F40 | 1830 | F180 | 1580 |
F46 | 1800 | F220 | 1500 |
F54 | 1780 | | |
Granulation compound of grains 99 A I b F12 to F 220 has to meet requirements FEPA standard 42-D-1984. After agreement there is also a possibility to supply grainmixtures in framework of technological possibilities.
Mehr auf:
KORUND Benátky s.r.o. |
|
CHROMOXID CR2O3 |
|
Chromoxide, Chromoxidgrün ist ein synthetisches Pigment mit einem hohen Gehalt an CR203. Dank des hohen Gehaltes an CR203 und der hohen Schmelztemperatur -2450 °C – wird dieses vor allem als Zusatzmittel in Feuerfestprodukten. |
Schmelztemperatur |
SILICIUMCARBID SiC |
2730 °C |
EDELKORUND WEIß Al2O3 |
2072 °C |
CHROMOXID Cr2O3 |
2275 °C |
Feuerfester Werkstoff |
Die Hauptkomponenten anorganischer nichtmetallischer Materialien (Keramik und Glas, Glaskeramik, Glasfasern und Mineralfasern) sind die Oxide Siliciumdioxid, Aluminiumoxid, Magnesiumoxid, Calciumoxid, Zirconiumoxid und Chromoxid. Zudem sind Kohlenstoff (C) und Siliciumcarbid (SiC) wichtige Komponenten. Außerdem muss man die sog. Refraktärmetalle (Molybdän, Wolfram) sowie die Platingruppenmetalle (Edelmetalle) und ihre Legierungen auf Grund ihrer hohen Schmelzpunkte und ihrer chemischen Beständigkeit gegenüber vielen Schlacken und Schmelzen zu den feuerfesten Werkstoffen zählen. |
|